MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Petropol Tenopom® B3 MF CNZ0522 PR360 MSP POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Product Description: Medium Flow, Copolymer, Polyoxymethylene (POM)

Resin ID (ISO 1043): POM
Processing: Injection Molding
Color: Gray

Information provided by Petropol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccASTM D792/A
Linear Mold Shrinkage, Flow 0.020 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0175 cm/cmASTM D955
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238/A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM D785
Tensile Strength 60.0 MPaASTM D638
Elongation at Break 35 %ASTM D638
Flexural Strength 88.0 MPaASTM D790
Flexural Modulus 2500 MPaASTM D790
Izod Impact, Notched 60.0 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D150
Dissipation Factor 0.0060ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 130 µm/m-°CASTM D696
Melting Point 170 °C
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °CASTM D648
Vicat Softening Point 162 °CASTM D1525
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 200 °CMolding
Mold Temperature 70.0 - 80.0 °C
Drying Temperature 80.0 °C
Dry Time 2.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPETROPOL387 / 313295

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.