MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Hi-Strength 90 Spray Adhesive-Low VOC <25%
Categories: Polymer; Adhesive

Material Notes: An industrial grade high strength aerosol spray adhesive.

Features:

  • Bonds to a variety of substrates including decorative laminate, headliners, and soft foams.
  • Typically used in construction, woodworking, specialty vehicle, RV, and manufactured housing
  • A high strength, fast, contact-type adhesive
  • Helps contribute to LEED® credits
  • GREENGUARD Indoor Air Quality Certified®

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.875 g/cc
Solids Content 23.2 %
 
Descriptive Properties
AppearanceClear
BaseSynthetic Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bostik Tube & Tile Caulk Siliconized-Acrylic Caulk
Lucite International Series 500 Liquid Acrylic Resin
Dow Everest™ 200 Latex Modified Acrylic Emulsion
BYK Optiflo® T1000 (Formerly RXL-7301) Polymer
Blue River Coatings Acrylic 4000 Topcoat

PMM34052 / 168799

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.