MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek Pyrocast XL Small Component Refractory
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Applications
  • Thimbles
  • Transition plates
  • Down Spouts
  • Control Pins
  • Auto pour Ladles
  • Strip Casting Nozzles

Advantages

  • Thermal shock resistance
  • High erosion resistance
  • High service temperature
  • Smooth cast surface
  • Dimensionally stable
  • Preheating unnecessary
  • Easily cleaned
  • Non-wetting

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.90 - 1.95 g/cc0.0686 - 0.0704 lb/in³
Open Porosity 22 - 23 %22 - 23 %
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.0140 GPa
@Treatment Temp. 725 °C
2.03 ksi
@Treatment Temp. 1340 °F
Compressive Strength 55.0 MPa7980 psicured at 725°C
 
Thermal PropertiesMetricEnglishComments
CTE, linear 0.820 µm/m-°C
@Temperature 200 - 700 °C
0.456 µin/in-°F
@Temperature 392 - 1290 °F
Thermal Conductivity  0.860 W/m-K
@Temperature 460 °C
5.97 BTU-in/hr-ft²-°F
@Temperature 860 °F
 0.880 W/m-K
@Temperature 610 °C
6.11 BTU-in/hr-ft²-°F
@Temperature 1130 °F
 0.930 W/m-K
@Temperature 790 °C
6.45 BTU-in/hr-ft²-°F
@Temperature 1450 °F
Maximum Service Temperature, Air 1000 °C1830 °F
Shrinkage -0.0770 %
@Temperature 700 °C
-0.0770 %
@Temperature 1290 °F
Linear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek Pyrocast SC-2600 Castable Refractory
Pyrotek Pyrocast HD Castable Refractory
Pyrotek Pyrocast TG Castable Refractory
Pyrotek Pyrocast SCM-2600 High Wear Impact Refractory Castable
Pyrotek Pyrocast SC-2600 Refractory Cast Parts

CPYRO176 / 1893

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.