MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ALM Ultrasint® PA6 LM Nylon 6, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Ultrasint PA6 LM is a special powder material designed to maximize production accessibility to any PBF user.

Highlights:

  • Low melting Polyamide 6-based powder for Laser Sintering
Applications:
  • Functional prototypes (i.e. in automotive industries)
  • High performance spare parts
  • Multi-purpose industrial goods
  • Durable and rigid jigs & fixtures

Information provided by Advanced Laser Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.590 g/ccDIN EN ISO 60
Density 1.37 g/ccPrinted Part; DIN EN ISO 1181-1
Particle Size 80 µmD50
Melt Flow 4.11 g/10 min
@Load 2.16 kg,
Temperature 240 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 32.0 MPa
@Temperature 80.0 °C
Z-Direction; ISO 527-2
 44.0 MPa
@Temperature 80.0 °C
X-Direction; ISO 527-2
 49.0 MPa
@Temperature 23.0 °C
Z-Direction; ISO 527-2
 73.0 MPa
@Temperature 23.0 °C
X-Direction; ISO 527-2
Elongation at Break 1.3 %
@Temperature 23.0 °C
Z-Direction; ISO 527-2
 2.8 %
@Temperature 23.0 °C
X-Direction; ISO 527-2
 6.5 %
@Temperature 80.0 °C
Z-Direction; ISO 527-2
 19 %
@Temperature 80.0 °C
X-Direction; ISO 527-2
Tensile Modulus 1100 MPa
@Temperature 80.0 °C
Z-Direction; ISO 527-2
 1250 MPa
@Temperature 80.0 °C
X-Direction; ISO 527-2
 4250 MPa
@Temperature 23.0 °C
Z-Direction; ISO 527-2
 4950 MPa
@Temperature 23.0 °C
X-Direction; ISO 527-2
Flexural Modulus 3650 MPaZ-Direction; DIN EN ISO 178
 4500 MPaX-Direction; DIN EN ISO 178
Izod Impact, Notched (ISO) 3.30 kJ/m²Z-Direction; ISO 180
 3.80 kJ/m²X-Direction; ISO 180
Izod Impact, Unnotched (ISO) 6.00 kJ/m²Z-Direction; ISO 180
 15.0 kJ/m²X-Direction; ISO 180
Charpy Impact Unnotched 5.70 kJ/m²Z-Direction; ISO 179-1
 18.0 kJ/m²X-Direction; ISO 179-1
Charpy Impact, Notched 2.80 kJ/m²Z-Direction; ISO 179-1
 3.00 kJ/m²X-Direction; ISO 179-1
 
Thermal PropertiesOriginal ValueComments
Melting Point 193 °CISO 11357
Crystallization Temperature 149 °CISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 183 °CISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °CISO 75-2
Vicat Softening Point 185 °C
@Load 5.10 kg
B; ISO 306
 194 °C
@Load 1.02 kg
A; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PALP9023 / 312358

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.