MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Viton® A-601C with MT Black Fluoroelastomer Compound
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes:
  • Fully precompounded for O-ring curative level
  • Improved processing for a high viscosity polymer with improved mold flow, easier mold release, and less mold fouling
  • Excellent scorch safety
  • Excellent physical properties for improved compression set resistance

Applications

  • Compression molding of O-rings, gaskets, and other sealing devices
  • Applications where a higher polymer viscosity is needed for molding operations. Can be used to modify viscosity of other types of Viton®.
  • Can be formulated to meet FKM specifications Mil-R-83248C and AMS 7276E.

Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 103
@Temperature 121 °C
ML (1+10), Uncompounded Viton; ASTM D1646
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 76ASTM D2240
Tensile Strength at Break 15.3 MPaASTM D412
Elongation at Break 219 %ASTM D412
100% Modulus 0.00640 GPa
@Strain 100 %
ASTM D412
Compression Set 6.0 %
@Temperature 200 °C,
Time 79200 sec
O-Rings; ASTM D395B
 6.0 %
@Temperature 23.0 °C,
Time 252000 sec
O-Rings; ASTM D395B
 9.0 %
@Temperature 200 °C,
Time 79200 sec
O-Rings; ASTM D395B
 11 %
@Temperature 200 °C,
Time 252000 sec
O-Rings; ASTM D395B
 21 %
@Temperature 200 °C,
Time 605000 sec
O-Rings; ASTM D395B
 31 %
@Temperature 232 °C,
Time 252000 sec
O-Rings; ASTM D395B
 
Processing PropertiesOriginal ValueComments
Processing Temperature 177 °C
@Time 601 sec
Slab Cure
 232 °C
@Time 86400 sec
Postcure
 
Descriptive Properties
Formulation as Tested100A-601C
 3MgO
 30MT Black
 6Ca(OH)2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Viton® A-601C with 15 MT Black Fluoroelastomer Compound
Chemours Viton® ETP-900 Fluoroelastomer (FKM)
Chemours Viton® A-401C Fluoroelastomer Compound
Chemours Viton® A-601C Fluoroelastomer Compound
Chemours Viton® A-601C with 60 MT Black Fluoroelastomer Compound

PDVC9934 / 170575

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.