Sequel 1514-UV 11BK thermoplastic polyolefin material exhibits significantly greater mar resistance than conventional TPOs. Sequel 1514-UV 11BK polyolefin is typically used for automotive applications that demand low warpage and low CLTE, along with excellent scratch and mar resistance. Applications: Automotive Parts, Exterior Automotive Applications.Information provided by LyondellBasell. |