MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Surlyn® 9020 Ionomer Resin, Zinc
Categories: Polymer; Thermoplastic; Ionomer; Ionomer, Molded

Material Notes: Surlyn® 9020 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The resin contains an additional co-monomer to facilitate its use as a modifier for toughened grades of nylon 6 and 6/6. The amount of MAA and neutralization levels for this grade are optimized to impart low-temperature toughness. The resin complies with the provisions of U.S. Food and Drug Administration (FDA) Title 21 Code of Regulations 177:1330 - ionomer resins.

Data provided by the manufacturer.

This former DuPont product line is now a Dow product line.

Key Words: Ethylene/Methacrylic Acid (E/MAA) Copolymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³ASTM D792
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
condition E; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555ASTM D2240
Tensile Strength, Ultimate 26.2 MPa3800 psiASTM D638
Elongation at Break 510 %510 %ASTM D638
Flexural Modulus 0.100 GPa14.5 ksiASTM D790
Izod Impact, Notched NBNBASTM D256
Tensile Impact Strength 1280 kJ/m²609 ft-lb/in²ASTM D1822S
Abrasion 220220NBS Index; ASTM D1630
 
Thermal PropertiesMetricEnglishComments
CTE, linear 170 µm/m-°C
@Temperature -20.0 - 32.0 °C
94.4 µin/in-°F
@Temperature -4.00 - 89.6 °F
ASTM D696
Thermal Conductivity 0.240 W/m-K1.67 BTU-in/hr-ft²-°F
Melting Point 81.0 °C178 °FDTA
Deflection Temperature at 0.46 MPa (66 psi) 40.0 °C104 °FASTM D648
Vicat Softening Point 57.0 °C135 °FRate B, ASTM D1525-70
Brittleness Temperature -112 °C-170 °FASTM D746
Flame Spread 25.4 mm/min1.00 in/minASTM D635
 
Optical PropertiesMetricEnglishComments
Haze 7.0 %
@Thickness 6.35 mm
7.0 %
@Thickness 0.250 in
ASTM D1003A
Gloss 45 %45 %20° per ASTM D523-6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Surlyn® 6320 Magnesium Ionomer
Dow Surlyn® 9320 Zinc Ionomer
Dow Surlyn® 8940 Ionomer Resin, Sodium
Dow Surlyn® 9520 Ionomer Resin, Zinc
Dow Surlyn® 9950 Ionomer Resin, Zinc

PDU412 / 33063

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.