MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chemical Concepts Chem-Set™ C-30 Marblemaster Dripless Seaming Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: ChemSet C-30 is a two-part methacrylate, super flexible, dripless/non-sag, low shrink, low exotherm, ultra violet light stable, non-yellowing hard surfacing adhesive designed for the nearly seamless bonding of Porcelain, Sintered Stone, Glass, Engineered Stone, Marble, Quartz, and Natural Stone products. Applications: Fabrication of mitered edges, laminations and deck seams on: NATURAL STONE, CERAMICS , SINTERED SURFACES, QUARTZ, GLASS AND MORE.

Advantages: Non Drip / No Sag , Flexible Adhesive, Auto-dispense system, Invisible seams, Pre-mixed in 15 natural stone colors, High strength, UV resistant, Trimmable, LOW VOC.

Combined at a ratio of 10:1 (10 parts resin, one part activator), ChemSet C-30 Marblemaster has a working time of 10 to 15 minutes, with a 5 to 10 minute De-Roping Time, and achieves nearly 90 percent of its ultimate strength in 45 to 60 minutes at room temperature curing. ChemSet C-30 Marblemaster offers a combination of high strength, stiffness, and toughness as well as the ability to bond very strongly to a wide variety of hard surface or inorganic materials. ChemSet C-30 Marblemaster permits the seasoned fabricator the opportunity to apply the adhesive to vertical surfaces, as well as horizontal surfaces, without dripping, and upon gelation, gives the fabricator an extended window (5 to 10 minutes) to de-rope, or trim with a single bladed straight edge razor blade, the excess from the stone slab without ripping the adhesive out of the joint, nor damaging the surface of the stone.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.930 - 1.05 g/ccAdhesive
Density 7.70 - 8.80 lb/galrelative, Adhesive
 8.60 lb/galmixed
pH 4.0 - 6.0Adhesive
 4.0 - 6.0Activator
Viscosity 75000 cPActivator
 200000 - 350000 cPAdhesive
Vapor Pressure <= 0.500 torr
@Temperature 20.0 °C
Activator
 28.0 torr
@Temperature 20.0 °C
Adhesive
 
Thermal PropertiesOriginal ValueComments
Melting Point -54.0 °FAdhesive
Boiling Point 212 °FAdhesive
 >= 550 °FActivator
Flash Point 50.0 °FAdhesive, Tag closed cup
 51.0 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 65.0 - 85.0 °F
Working Life 10.0 - 12.0 min
Shelf Life 24.0 Month
 
Descriptive Properties
Auto Ignition Temperature790°FAdhesive
Chemical ResistanceHydrocarbons, Acids and Bases, Vinegar, Wine and condiments, Most household foods.
Chemical SusceptibilityPolar solvents, Super strong acids and bases.
ColorColorless, translucent, activator
 Various, adhesive
De-Roping Time (minutes)5 - 10
Evaporation Point<1 (butyl acetate =1). Activator
 3. Adhesive
Fixture Time20 - 30 minutes
Flammability TestClass 1B (activator)
 Class 1B (adhesive)
Gap Filling0.25 inches
Mix Ratio10 : 1
Routable (minutes)45 - 60
Vapor Density3.5 (air=1), Adhesive

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHEMI934 / 232164

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.