MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Radici RADILON® S RV250 100 NT Nylon 6, 25% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Description: PA6 25% glass fiber reinforced injection molding grade. Natural color. Suitable for parts requiring medium stiffness and good mechanical resistance.

Processing: Injection Molding

Delivery Form: Granules

Additives: Release agent

Special Characteristics: UL Listed

Industries: Consumer Industry Goods, Transportation

Regional Availability: North America, Europe, Asia Pacific, South and Central America, Near East/Africa

Information provided by Radici Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³ISO 1183
Water Absorption 7.5 %
@Thickness 2.00 mm
7.5 %
@Thickness 0.0787 in
Immersion at 23°C; ISO 62
Moisture Absorption 2.20 %
@Thickness 2.00 mm
2.20 %
@Thickness 0.0787 in
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inMelt Temp/Mold Temp/Cavity Pressure: 280/80/60; ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inMelt Temp/Mold Temp/Cavity Pressure: 280/80/60; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 165 MPa23900 psi5mm/min; ISO 527-2/1A
Tensile Stress  50.0 MPa
@Strain 0.5 %
7250 psi
@Strain 0.5 %
Break
 100 MPa
@Strain 1.1 %
14500 psi
@Strain 1.1 %
Break
 120 MPa
@Strain 3 %
17400 psi
@Strain 3 %
Break
 150 MPa
@Strain 2.1 %
21800 psi
@Strain 2.1 %
Break
Elongation at Break 4.0 %4.0 %5mm/min; ISO 527-2/1A
Tensile Modulus 8.10 GPa1170 ksi1mm/min; ISO 527-2/1A
Flexural Strength 245 MPa35500 psi2mm/min; ISO 178
Flexural Modulus 7.20 GPa1040 ksi2mm/min; ISO 178
Secant Modulus  7.40 GPa
@Strain 2 %
1070 ksi
@Strain 2 %
Break
 10.0 GPa
@Strain 0.25 %
1450 ksi
@Strain 0.25 %
Break
 14.6 GPa
@Strain 0.05 %
2120 ksi
@Strain 0.05 %
Break
Charpy Impact Unnotched  6.50 J/cm²
@Temperature -30.0 °C
30.9 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 8.50 J/cm²
@Temperature 23.0 °C
40.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.10 J/cm²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.30 J/cm²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cm500V; IEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohm500V; IEC 60093
Comparative Tracking Index 600 V600 VSol. A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 195 °C383 °FISO 75/2Af
Vicat Softening Point 210 °C
@Load 5.10 kg
410 °F
@Load 11.2 lb
50°C/h; ISO 306
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
Flame Spread <= 0.000 mm/min
@Thickness 3.00 mm
<= 0.000 in/min
@Thickness 0.118 in
Automotive Interior; ISO 3795
Glow Wire Flammability Index 700 °C
@Thickness 2.00 mm
1290 °F
@Thickness 0.0787 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 280 °C464 - 536 °F
Mold Temperature 80.0 - 90.0 °C176 - 194 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADICI131 / 313632

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.