MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Teknor Apex Elexar® EL-1934H Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Elexar EL-1934H is a high performance thermoplastic elastomer designed for electrical applications requiring flexibility over a wide temperature range. Elaxar EL-1934H is a low hardness, high density, RoHS compliant grade suitable for both injection molding and extrusion.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Filled; Flame Retardant; Good Flow; High Density; High Specific Gravity; Light Stabilized; Low Hardness; Lubricated; Medium Flow

Uses: Appliance Wire Insulation; Appliance Wire Jacketing. Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire & Cable Applications; Wire Jacketing

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.26 g/ccASTM D792
Melt Flow 25 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 35
@Time 5.00 sec
Injection Molded; ASTM D2240
 37
@Time 1.00 sec
Injection Molded; ASTM D2240
Tensile Strength at Break 400 psiDie C, 20 in/min, Flow; ASTM D412
 536 psiDie C, 20 in/min, Across Flow; ASTM D412
Tensile Stress at Strain 109 psi
@Strain 100 %
Die C, 20 in/min, Across Flow; ASTM D412
 151 psi
@Strain 100 %
Die C, 20 in/min, Flow; ASTM D412
 174 psi
@Strain 300 %
Die C, 20 in/min, Across Flow; ASTM D412
 228 psi
@Strain 300 %
Die C, 20 in/min, Flow; ASTM D412
Elongation at Break 640 %Die C, 20 in/min, Flow; ASTM D412
 760 %Die C, 20 in/min, Across Flow; ASTM D412
Tear Strength 80.0 pliDie C, 20 in/min, Flow; ASTM D624
 88.0 pliDie C, 20 in/min, Across Flow; ASTM D624
Compression Set 16 %
@Temperature 22.8 °C,
Time 79200 sec
Type I; ASTM D395B
 47 %
@Temperature 70.0 °C,
Time 79200 sec
Type I; ASTM D395B
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0
@Thickness 3.05 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 380 - 420 °FMelt, Injection
Rear Barrel Temperature 380 - 420 °FInjection
Middle Barrel Temperature 380 - 420 °FInjection
Front Barrel Temperature 380 - 420 °FInjection
Nozzle Temperature 380 - 420 °FInjection
Zone 1 360 - 400 °FExtrusion
Zone 2 360 - 400 °FExtrusion
Zone 3 360 - 400 °FExtrusion
Zone 4 360 - 400 °FExtrusion
Zone 5 360 - 400 °FExtrusion
Die Temperature 360 - 400 °FExtrusion
Mold Temperature 60.0 - 90.0 °FInjection
Injection Pressure 200 - 1000 psi
Back Pressure 25.0 - 50.0 psiInjection
Cushion 0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpmExtrusion
 50 - 100 rpmInjection
 
Descriptive Properties
AppearanceBlack
 Colors Available
 Natural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Medalist® MD-305 Thermoplastic Elastomer
Teknor Apex Medalist® MD-300 Thermoplastic Elastomer
Teknor Apex Medalist® MD-210 Thermoplastic Elastomer
Teknor Apex Medalist® MD-205 Thermoplastic Elastomer
Teknor Apex Medalist® MD-12170 Thermoplastic Elastomer

PTEKNQ0629 / 237120

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.