MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Petromont 2200 High Density Polyethylene Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Pétromont HDPE 2200 is a high-density polyethylene homopolymer resin produced using the UNIPOL® Process. This resin can be used in a mono layer or co-extrusion resin in applications requiring improved film stiffness and barrier properties, such as in Deli Wrap, cereal box liner, etc.

Pétromont HDPE 2200 is an intermediate molecular weight resin offering an excellent combination of maximum barrier properties and stiffness with no detectable taste and odour as well as good extrusion characteristics.

Key Words: Film extrusion, barrier properties
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.961 g/ccASTM D1505
Water Vapor Transmission 4.30 g/m²/day
@Temperature 37.8 °C,
Time 86400 sec
90% R.H.; ASTM E96
Oxygen Transmission 0.00450 cc-mm/m²-24hr-atmDry; ASTM D1434
Nitrogen Transmission 0.00160 cc-mm/m²-24hr-atmDry; ASTM D1434
Carbon Dioxide Transmission 0.0240 cc-mm/m²-24hr-atmDry; ASTM D1434
Melt Flow 0.70 g/10 minI2; ASTM D1238
 50 g/10 minI21; ASTM D238
 
Thermal PropertiesOriginal ValueComments
Melting Point 133 °CPetromont
Crystallization Temperature 119 °CPetromont
Vicat Softening Point 130 °CASTM D1525
 
Descriptive Properties
ProcessFilm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Global MB-6366 High Density Polyethylene
Global B-8200 High Density Polyethylene
AdvanSix Aegis® OX High Barrier Nylon
Nurel Engineering Polymers Promyde® B40 L PA 6, Dry, Lubricated
LyondellBasell Alathon 8005M-3 High Denisty Polyethylene

PPETROM09 / 56203

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.