MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Southern Polymer PRIMALENE® WPP502B Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: A fractional melt low density polypropylene

Typical Applications:

  • Agricultural film
  • Construction film
  • Heavy duty bags
  • Pallet shrink film
  • Zipper bags
Features:
  • Excellent strength properties
  • Outstanding processability
  • Slip: zero
  • Anti-block: 4000 ppm

Information provided by Southern Polymer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.919 g/ccASTM D792
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 4000 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1260 psiASTM D882
Film Tensile Strength at Yield, TD 1310 psiASTM D882
Film Elongation at Break, MD 430 %ASTM D882
Film Elongation at Break, TD 610 %ASTM D882
Elmendorf Tear Strength MD 610 gASTM D1922
Elmendorf Tear Strength TD 640 gASTM D1922
Dart Drop Test 600 gASTM D1709A
Film Tensile Strength at Break, MD 2600 psiASTM D882
Film Tensile Strength at Break, TD 2990 psiASTM D882
1% Secant Modulus, MD 23000 psiASTM D882
1% Secant Modulus, TD 24100 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 230 °FPeak
 
Optical PropertiesOriginal ValueComments
Haze 15 %ASTM D1003
Gloss 50 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOUTH021 / 283877

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.