MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

(Viewing data as-entered. Click here to return)
Cookson Group Plaskon® 7115 Conventional Encapsulant  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Molding Compound

Material Notes: This material is a standard epoxy molding compound used for the encapsulation of a variety of semiconductor devices ranging from small lead count DIPs to medium lead count PLCCs, to Transistors and SOICs. It was especially developed for balanced end use properties.

Features

  • Excellent moldability
  • Superior cosmetics
  • Improved markability
  • Outstanding device reliability

Information provided by Cookson Electronics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.89 g/cc
Linear Mold Shrinkage 0.0050 cm/cm
Spiral Flow 77.0 cmat 177°C and 1000 psi
Ash 72 %
Storage Temperature <= 5.00 °CRecommended
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85Cull hot, 90 sec @ 175°C
Flexural Strength 19998 psi
Flexural Modulus 1.9998e+6 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cm
Dielectric Constant 3.5
@Frequency 1000 Hz
Dielectric Strength 500 V/mil
Dissipation Factor 0.010
@Frequency 1000 Hz
Arc Resistance 180 sec110V AC
 
Thermal PropertiesOriginal ValueComments
CTE, linear 22.0 µm/m-°C
@Temperature 20.0 °C
Alpha 1
 63.0 µm/m-°C
@Temperature 20.0 °C
Alpha 2
Thermal Conductivity 0.8368 W/m-K
Glass Transition Temp, Tg 165 °C
Flammability, UL94 V-0
@Thickness 3.17 mm
 
Processing PropertiesOriginal ValueComments
Mold Temperature 170 - 190 °C
Back Pressure 1000 psi
Cure Time 4.00 hour
@Temperature 175 °C
Post mold
 60.0 - 90.0 sec
@Temperature 177 °C
Gel Time 0.267 minRam follower, at 177°C
Shelf Life 0.0670 Monthat 35°C, <40% loss of spiral flow
 0.100 Monthat 21°C, <40% loss of spiral flow
 24.0 Monthat 5°C, <40% loss of spiral flow
 
Descriptive Properties
Hydrolyzable Cl10 ppm
Preheat Temperature90-100°C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Molding Compound
Cookson Group Plaskon® LS-16 Low Stress Epoxy Molding Compound
Cookson Group Plaskon® CMU-870-2C Molded Underfill Compound for Flip Chip BGAs and CSPs
Cookson Group Plaskon® CMU-870-2B Molded Underfill Compound for Flip Chip BGAs and CSPs
Cookson Group Plaskon® CMU-870-2A Molded Underfill Compound for Flip Chip BGAs and CSPs

PPLASK026 / 56316

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.