MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chosun Refractories CH-S Hard Fireclay brick
Categories: Ceramic

Material Notes:

Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 2.32 g/cc
Porosity 17 %
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 500 kg(f)/cm²Cold Crushing Strength
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.80 µm/m-°C
@Temperature 1000 °C
Shrinkage -0.200 - 0.20 %
@Temperature 1350 °C,
Time 7200 sec
 
Component Elements PropertiesOriginal ValueComments
Al2O3 43 %
Fe2O3 1.5 %
 
Descriptive Properties
QualityAnti-abrasion, Anti-spalling
Refractories Under Load(2kg/cm²,T2°C)1,450
Refractoriness (SK)34

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman POLYBATCH™ White P8555 T2 Concentrate Based In Homopolymer Polypropylene
A. Schulman POLYBATCH™ White 8000 AP Concentrate Based In LDPE
Concrete, clinker aggregate
Chosun Refractories SF-S Hard Fireclay brick
Chosun Refractories N5 Fireclay brick

CCHOS036 / 123980

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.