MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials Stat-Rite® S1100 TPU Alloy
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Product Description: S1100 is a static dissipative TPU alloy. It utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. Stat-Rite® IDP alloys provide consistent static dissipation even when extruded, injection molded or thermoformed into components.
Availability: Asia Pacific, Europe, Latin America, North America
Additive: Antistatic
Features: Antistatic; Copolymer; Durable; ESD Protection; Good Colorability; Humidity Resistant; Low (to None) Ion Content; Low to No Outgassing
Uses: Conveyor Parts; Electrical/Electronic Applications; Film; Hose; Rollers; Tubing
Appearance: Clear/Transparent; Light Blue
Forms: Pellets
Processing Method: Extrusion; Injection Molding; Thermoforming

Information provided by Lubrizol Advanced Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90ASTM D2240
Hardness, Shore D 47ASTM D2240
Tensile Strength at Break 3770 psiASTM D412
Tensile Stress 1160 psi
@Strain 100 %
ASTM D412
 2180 psi
@Strain 300 %
ASTM D412
Elongation at Break 450 %ASTM D412
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+9 ohm-cmASTM D257
Surface Resistance 5.00e+8 ohm12% RH; ESD S11.11
 5.00e+9 ohm50% RH; ASTM D257
Static Decay 0.010 sec5000 V to 50 V, FTMS-101C, 12% RH
 0.010 sec-5000 V to -50 V, FTMS-101C, 12% RH
 0.10 sec1000 V to 10 V, Charged Plate Monitor, 50% RH
 
Descriptive Properties
Ionic Content<2 ng/cm2Anion Br
 1 ng/cm2Anion F
 10 ng/cm2Anions NO3
 10 ng/cm2Anions SO4
 50 ng/cm2Anions PO4
 6 ng/cm2Anion Cl
Outgassing<0.02 µg/gStyrene
 <0.02 µg/gToluene
 0.04 µg/gMMA
 4.5 µg/gTotal Organics

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLUBR6018 / 268320

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.