MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
UBE UBEPOL BR150L Synthetic Rubber (Compound)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: UBEPOL BR is UBE's line of polybutadiene rubber products.

Information provided by UBE.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 54.2
@Temperature 100 °C
ML1+4; ASTM D1646
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 0.480 MPa
Elongation at Break 1290 %
Modulus of Elasticity 0.000230 GPa600% Modulus
50% Modulus 0.000220 GPa
@Strain 50 %
300% Modulus 0.000200 GPa
@Strain 300 %
 
Thermal PropertiesOriginal ValueComments
Shrinkage 44 %Mill Shrinkage
 
Processing PropertiesOriginal ValueComments
Extrusion Rate 74.5 g/min
Cure Time 10.1 mint10
 12.6 mint90
 
Descriptive Properties
Die Swell4.32 g/min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
UBE UBEPOL VCR412 Synthetic Rubber (Raw Polymer)
UBE UBEPOL VCR303 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
UBE UBEPOL BR150B Synthetic Rubber (Compound)
UBE UBEPOL BR150 Non-Oil Extended Synthetic Rubber (Raw Polymer)
Lanxess Perbunan® 3976 VP Synthetic Rubber

PUBE187 / 71747

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.