MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyram Bondyram® 1001CN Maleic Anhydride Modified Co-Polymer Propylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Recommended for coupling of glass and other fillers in polypropylene composites.

Information provided by Polyram.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183
Melt Flow 100 g/10 min
@Load 2.13 kg,
Temperature 190 °C
100 g/10 min
@Load 4.70 lb,
Temperature 374 °F
ISO 1133
 
Thermal PropertiesMetricEnglishComments
Melting Point 167 °C333 °FISO 11357

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyram Bondyram® TL1207 Maleic Anhydride Modified Co-Polymer Polypropylene
Polyram Bondyram® 1101 Maleic Anhydride Modified Homo Propylene
Polyram BondyRam® 1001 Maleic Anhydride modified Homo-polypropylene coupling agent
Polyram Bondyram® 4108 Maleic Anhydride Modified Linear Low Density Polyethylene
Polyram Bondyram® 7103 Maleic Anhydride Modified Ethylene-Alpha Olefin Copolymer

PPOLYR876 / 126675

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.