MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis FG5199 Linear Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: FG5199 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes antioxidant, anti-Fog and cling additives. The grade is developed for blown cling film. Film made from FG5199 is suitable for manual wrapping of various foodstuffs e.g. cheese, meat and vegetables. Applications: cling, food packaging, food wrap film, and lamination films.

Information provided by Borealis AG

Key Words: LLDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.919 g/ccISO 1183
Melt Flow 1.25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 11.0 MPaTD; ISO 527-3
Film Elongation at Break, MD 550 %ISO 527-3
Film Elongation at Break, TD 710 %ISO 527-3
Elmendorf Tear Strength, MD 2.04 g/micronISO 6383/2
Elmendorf Tear Strength, TD 15.49 g/micronISO 6383/2
Dart Drop Test 70.0 g
@Thickness 0.0250 mm
ISO 7765-1
Film Tensile Strength at Break, MD 32.0 MPaISO 527-3
Film Tensile Strength at Break, TD 28.0 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 121 °CISO 11357-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Borstar® FB2230 LLDPE for Film
Borealis FG5224 Linear Low Density Polyethylene
Borealis FG5190 Linear Low Density Polyethylene
Borealis FG5223 Linear Low Density Polyethylene
A. Schulman CP814-01 Linear, Low-Density Polyethylene

PBOREA440 / 108699

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.