MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow AFFINITY™ SM 1350 Polyolefin Plastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: AFFINITY® SM 1350 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in durable injection molded housewares and compression molded closure liners or gaskets. It exhibits good optics and flexibility. It can be used in hot fill applications and allows the use of hot runner molds to enhance production automation. Its low specific gravity can help control resin and production costs, while reducing the weight of end products.

Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.913 g/cc
Melt Flow 30 g/10 min
@Load 2.16 kg
Melt flow ratio I10/I2 is 7.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 96
Tensile Strength, Yield 8.30 MPa
Elongation at Break 700 %
Modulus of Elasticity 0.178 GPaMolded Sample 2% Secant Modulus
Flexural Modulus 0.239 GPa
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 88.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow AFFINITY™ EG 8150 Polyolefin Elastomer
Dow AFFINITY™ SM 8400 Polyolefin Elastomer
Dow AFFINITY™ SE 1400 Polyolefin Plastomer
Dow AFFINITY™ SM 1300 Polyolefin Plastomer
Dow AFFINITY™ SM 8250 Polyolefin Plastomer

PDW410 / 34479

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.