MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF Ultradur® S 4090 GX 14% Glass Filled PBT + ASA
Categories: Polymer; Thermoplastic; ASA Polymer; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + ASA Blend, Glass Fiber Reinforced

Material Notes: PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 14% of glass fibers for industrial parts with high dimensional stability, for example internal components for vehicles, plug connectors and housings.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.33 g/ccISO 1183
Moisture Absorption at Equilibrium 0.20 %23°C; 50% RH
Water Absorption at Saturation 0.40 %DIN 53495/1L
Viscosity Measurement 70
@Temperature 290 °C
20 mins plasticating
 75
@Temperature 300 °C
10 mins plasticating
 75
@Temperature 280 °C
30 mins plasticating
 90
@Temperature 270 °C
30 mins plasticating
 95
@Temperature 290 °C
10 mins plasticating
 100
@Temperature 300 °C
5 mins plasticating
 100
@Temperature 260 °C
30 mins plasticating
 105
@Temperature 280 °C
10 mins plasticating
 106
@Temperature 250 °C
30 mins plasticating
 110
@Temperature 270 °C
10 mins plasticating
 115
@Temperature 260 °C
10 mins plasticating
 115
@Temperature 240 °C
30 mins plasticating
 117
@Temperature 250 °C
10 mins plasticating
 120
@Temperature 240 °C
10 mins plasticating
Viscosity Test 110 cm³/gViscosity number; ISO 1628
Linear Mold Shrinkage, Flow 0.0032 cm/cmSheet
 0.0054 cm/cm60x60x2 mm; ISO 294
Linear Mold Shrinkage, Transverse 0.0083 cm/cm60x60x2 mm; ISO 294
 0.0099 cm/cmSheet
Melt Flow 30.59 g/10 min
@Load 2.16 kg,
Temperature 275 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 100 MPa50 mm/min; ISO 527-2
Elongation at Yield 3.2 %50 mm/min; ISO 527-2
Modulus of Elasticity 5.50 GPaISO 527-2
Flexural Strength 140 MPaISO 178
Charpy Impact Unnotched 52.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 9.50e+15 ohm-cmIEC 93
Surface Resistance >= 5.00e+15 ohmIEC 93
Dielectric Constant 3.4
@Frequency 1e+6 Hz
IEC 250
 3.6
@Frequency 100 Hz
IEC 250
Dissipation Factor 0.0039
@Frequency 100 Hz
IEC 250
 0.0208
@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 375 VTest solution A; IEC 112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 52.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
DIN 53752
Melting Point 220 - 225 °CDSC; ISO 11357-3
Maximum Service Temperature, Air 170 °C
Deflection Temperature at 0.46 MPa (66 psi) 210 °CISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 170 °CISO 75-2
Decomposition Temperature >= 300 °C
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Diameter 0.800 mm
Ignition Temperature >= 400 °CASTM D1929
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 °CHopper Throat
Zone 1 260 °CFeeding zone
Zone 2 265 °CCompression
Zone 3 270 °CMetering-zone
Zone 4 270 °CNozzle
Melt Temperature 250 - 280 °CInjection-molding
 270 °Cfor shrinkage test, Optimal
Mold Temperature 60.0 - 100 °C
 80.0 °Cfor shrinkage test, Optimal
Drying Temperature 80.0 - 120 °C
Dry Time 4 hour
 
Descriptive Properties
ColorNatural and Black
Commercial StatusEurope
Peripheral Screw Speed< 0.25 m/s
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultradur® B 4406 G6 30% Glass Filled PBT
BASF Ultradur® S 4090 GM13 5/15% Glass/Mineral Filled PBT + ASA
BASF Ultradur® B 4300 M2 12.5% Mineral Filled PBT
BASF Ultradur® B 4300 K6 30% Glass Bead Filled PBT
BASF Ultradur® B 4300 K4 20% Glass Bead Filled PBT

PBASG0098 / 131732

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.