MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ DP8010NS Structural Adhesive
Categories: Polymer; Adhesive

Material Notes: 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropylene, Polyethylene, and TPO’s with out special surface preparation. It can replace screws, rivet, plastic welding, and two-step processes which include chemical etchants, priming or surface treatments in many applications. DP-8010NS is a non-sag product designed to be used in applications where a high viscosity product is needed such as a vertical surface.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 27000 cPAccelerator, DV-II, #7 sp, 20 rpm
 70000 cPBase, DV-II, #7 sp, 20 rpm
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 50.0 psiOverlap, Toluene for 14 days, Cohesive Failure
 125 psiOverlap, Al/HDPE (non-abraded aluminum), Adhesive Failure to Al
 150 psiOverlap, Acetal, Adhesive Failure
 275 psiOverlap, Acetone for 14 days, Cohesive Failure
 400 psiOverlap, LDPE, Substrate Failure
 475 psiOverlap, PTFE, Adhesive Failure
 575 psiOverlap, HIPS, Substrate Failure
 575 psiOverlap, Gasoline for 14 days, Cohesive Failure
 600 psiOverlap, Glass (3/16" thick), Substrate Failure
 600 psiOverlap, RK8010A Top Coat CRS/HDPE, Adhesive Failure
 750 psiOverlap, Polystyrene, Substrate Failure
 775 psiOverlap, UHMWPE, Substrate Failure
 850 psiOverlap, CRS/HDPE, Adhesive Failure to CRS
 875 psiOverlap, HCl for 14 days, Substrate Failure
 875 psiOverlap, Isopropyl Alcohol for 14 days, Substrate Failure
 900 psiOverlap, 71°C/100% RH for 14 days, AF/CF
 925 psiOverlap, Diesel Fuel for 14 days, Substrate Failure
 950 psiOverlap, PE, Substrate Failure
 950 psiOverlap, DCT 5002X Top Coat CRS/HDPE (non-abraded CRS), AF/Top Coat
 950 psiOverlap, NaOH for 14 days, Substrate Failure
 975 psiOverlap, Antifreeze Coolant for 14 days, Substrate Failure
 1025 psiOverlap, ED-5000 E-Coated CRS/HDPE, Adhesive Failure
 1050 psiOverlap, Lexan, AF/CF
 1100 psiOverlap, HDPE, Substrate Failure
 1100 psiOverlap, Control, Substrate Failure
 1150 psiOverlap, PP, Substrate Failure
 1150 psiOverlap, Plexiglas (PMMA), Substrate Failure
 1175 psiOverlap, 71°C water soak for 14 days, Cohesive Failure
 1200 psiOverlap, 304 Stainless Steel (1/32" thick), Adhesive Failure
 1375 psiOverlap, EC 3924 Primed CRS (non-abraded CRS), AF/CF
 1450 psiOverlap, Gel Coat (3/16" thick), Substrate Failure
 1475 psiOverlap, ABS, Substrate Failure
 1500 psiOverlap, EC 3924 Primed Al/HDPE (non-abraded Al), Cohesive Failure
 1875 psiOverlap, Copper (1/16" thick), AF/CF
 1950 psiOverlap, Aluminum (1/16" thick), Adhesive Failure
 2050 psiOverlap, PVC, Substrate Failure
 2050 psiOverlap, CRS (1/32" thick), Adhesive Failure
 2525 psiOverlap, Green FRP, AF/CF
 400 psi
@Temperature 82.0 °C
Overlap
 2400 psi
@Temperature 24.0 °C
Overlap
Peel Strength 30.0 pliT-Peel
 30.0 pliT-Peel, HDPE, Substrate Failure
 
Thermal PropertiesOriginal ValueComments
CTE, linear 132 µm/m-°CBelow Tg
 207 µm/m-°CAbove Tg
Glass Transition Temp, Tg 34.0 °Conset
 
Processing PropertiesOriginal ValueComments
Cure Time 1.50 - 2.00 hourTime to Handling Strength
 8.00 - 24.0 hourFull Cure
 
Descriptive Properties
AppearancePink/AmberBase
 WhiteAccelerator
 Yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ DP8010 Structural Adhesive
Silberline SilBerCote® PC 3331X

PMM34671 / 169418

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.