MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Norplex-Micarta EndurX™ BP18NPA Phenolic Canvas Laminate Sheet
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic

Material Notes: BP11NPA is a red colored composite made from a 24 oz/sq. yd canvas which is passed through the treater twice to insure impregnation of the fibers and to obtain the resin content desired for optimal performance. The resin system is a phenolic with good impregnation qualities and cured hardness. BP11NPA is designed for highly loaded bearing applications, where the lubrication is provided by oil, water or a mixture.

Key Words: Cotton, Phenolic, Micarta
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.42 g/cc1.42 g/ccASTM D792
Moisture Absorption 0.0600 %0.0600 %Condition A; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9595ASTM D785
Tensile Strength  77.9 MPa
@Thickness 12.7 mm
11300 psi
@Thickness 0.500 in
Condition A, Crosswise; ASTM D638
 78.6 MPa
@Thickness 12.7 mm
11400 psi
@Thickness 0.500 in
Condition A, Lengthwise; ASTM D638
Flexural Strength  93.8 MPa
@Thickness 12.7 mm
13600 psi
@Thickness 0.500 in
Condition A, Crosswise; ASTM D790
 139 MPa
@Thickness 12.7 mm
20200 psi
@Thickness 0.500 in
Condition A, Lengthwise; ASTM D790
Flexural Modulus  7.129 GPa
@Thickness 12.7 mm
1034 ksi
@Thickness 0.500 in
Condition A, Crosswise; ASTM D790
 9.363 GPa
@Thickness 12.7 mm
1358 ksi
@Thickness 0.500 in
Condition A, Lengthwise; ASTM D790
Compressive Strength 252 MPa
@Thickness 12.7 mm
36500 psi
@Thickness 0.500 in
Condition A, Flatwise; ASTM D695
Shear Strength 95.8 MPa
@Thickness 12.7 mm
13900 psi
@Thickness 0.500 in
Condition A, Perpendicular; ASTM D732
Adhesive Bond Strength 15.9 MPa
@Thickness 12.7 mm
2300 psi
@Thickness 0.500 in
Condition A, Bonding Strength; ASTM D229
Izod Impact, Notched  1.51 J/cm
@Thickness 12.7 mm
2.83 ft-lb/in
@Thickness 0.500 in
Condition E-48/50, Crosswise; ASTM D256
 3.40 J/cm
@Thickness 12.7 mm
6.36 ft-lb/in
@Thickness 0.500 in
Condition E-48/50, Lengthwise; ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.5 µm/m-°C10.8 µin/in-°FX-axis; IPC-TM 650-2.4.24
 27.6 µm/m-°C
@Thickness 12.7 mm
15.3 µin/in-°F
@Thickness 0.500 in
Y-axis; IPC-TM 650-2.4.24
UL RTI, Mechanical without Impact 125 °C257 °FUL Bulletin 746b
Flammability, UL94 HB
@Thickness 12.7 mm
HB
@Thickness 0.500 in
Condition A
 
Descriptive Properties
SubstrateCotton

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNORPM241 / 280557

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.