Application: High-flow flame retardant TPO compound for insulation and jacketing designed for ribbon cable applications. The flame retardant package incorporates non-PDBPO, PBB, PBDE flame retardants, which is RoHS and WEEE compliant. The GTPO8102BA-H series of products is formulated to meet UL VW-1 testing as well as the CSA test C22-2 No. 0.6 flame test.Information provided by S&E Specialty Polymers; S&E Specialty Polymers was aquired by Aurora Plastics in 2017. |