MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Arlon Electronic Materials 51N Lead-Free Compatible Epoxy Low-Flow
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: 51N is a non-DICY multifunctional epoxy low-flow prepreg system designed to provide high reliability through lead-free solder operations. The high decomposition temperature and high thermal stability of this material is ideal for use in complex rigid-flex fabrication and assembly operations where minimum resin flow is required.

  • Decomposition Temperature > 350°C is ideally suited for lead-free solder processing and offers significant improvement over traditional FR-4 Epoxy systems.
  • Multifunctional epoxy resin system with a Glass transition temperature of 170°C thermal cycling PTH reliability
  • Improved bond adhesion over multiple thermal excursions results in better reliability through reflow and rework operations.
  • Electrical and mechanical properties meet the flow requirements of IPC-4101B/124 prepreg, modified to be low-flow.
  • Compatible with lead-free solder processing
  • RoHS/WEEE compliant

Typical Applications:

  • Bonding multilayer rigid-flex boards
  • Attaching heat sinks to finished PCB assemblies
  • Dielectric insulators
  • Other applications where minimal and uniform resin flow is required

    Information provided by ARLON Electronic Materials.

  • Vendors: Arlon Materials for Electronics (MED) is a major manufacturer of specialty high performance laminate and prepreg materials for use in a wide variety of printed circuit board (PCB) applications and in several distinctive markets.

    Click here to view all available suppliers for this material.

    Please click here if you are a supplier and would like information on how to add your listing to this material.

     
    Physical PropertiesOriginal ValueComments
    Density 1.35 g/ccASTM D792 Method A
    Water Absorption 0.15 %IPC TM-650 2.6.2.1
     
    Mechanical PropertiesOriginal ValueComments
    Tensile Strength 6500 psiIPC TM-650 2.4.18.3
    Modulus of Elasticity 2600 ksiIPC TM-650 2.4.18.3
    Flexural Strength 84.0 ksiIPC TM-650 2.4.4
    Peel Strength 6.40 pliTo Copper (1 oz./35 micron); After Process Solutions; IPC TM-650 2.4.8
     6.70 pliTo Copper (1 oz./35 micron); After Thermal Stress; IPC TM-650 2.4.8
     6.70 pliTo Copper (1 oz./35 micron); At Elevated Temperatures; IPC TM-650 2.4.8.2
     
    Electrical PropertiesOriginal ValueComments
    Volume Resistivity 2.60e+13 ohm-cmC96/35/90; IPC TM-650 2.5.17.1
     3.30e+13 ohm-cmE24/125; IPC TM-650 2.5.17.1
    Surface Resistance 4.00e+12 ohmE24/125; IPC TM-650 2.5.17.1
     2.90e+13 ohmC96/35/90; IPC TM-650 2.5.17.1
    Dielectric Constant 4.1
    @Frequency 1e+9 Hz
    may vary with resin %; IPC TM-650 2.5.5.9
     4.2
    @Frequency 1e+6 Hz
    may vary with resin %; IPC TM-650 2.5.5.3
    Dielectric Strength 1000 V/milIPC TM-650 2.5.6.2
    Dissipation Factor 0.020
    @Frequency 1e+6 Hz
    IPC TM-650 2.5.5.3
     0.020
    @Frequency 1e+9 Hz
    IPC TM-650 2.5.5.9
    Arc Resistance >= 120 secIPC TM-650 2.5.1
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear 14.0 µm/m-°CIPC TM-650 2.4.41
    CTE, linear, Transverse to Flow 44.0 µm/m-°Cz, below Tg; IPC TM-650 2.4.24
     245 µm/m-°Cz, above Tg; IPC TM-650 2.4.24
    Thermal Conductivity 0.250 W/m-KASTM E1461
    Glass Transition Temp, Tg 166 °CTMA; IPC TM-650 2.4.24
     170 °CDSC; IPC TM-650 2.4.25
    Decomposition Temperature 354 °COnset; IPC TM-650 2.4.24.6
     368 °C5 percent; IPC TM-650 2.4.24.6
    Flammability, UL94 V-0
     
    Descriptive Properties
    IPC Delamination - T260 (minutes)> 60IPC TM-650 2.4.24.1
    IPC Delamination - T288 (minutes)> 30IPC TM-650 2.4.24.1
    IPC Delamination - T300 (minutes)15IPC TM-650 2.4.24.1
    Z-Axis Expansion (%)2.6IPC TM-650 2.4.24 (50-260°C)

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Overview of materials for Epoxy Cure Resin
    Aremco Aremco-Bond™ 526N High Performance Epoxide

    PARLM9875 / 149028

    Ensinger PEI

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.