MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wieland 1951 Wilaform Platinum
Categories: Metal; Nonferrous Metal; Precious Metal; Platinum Alloy

Material Notes: Platinum alloy for technical use.

Applications: casting, chains, laminar decoration, pipes, tubing

Dental

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 21.6 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 105HV5; glowed
Tensile Strength, Ultimate 340 MPa
Elongation at Break 2.0 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 1790 - 1800 °C
Solidus 1790 °C
Liquidus 1800 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1832 °FCuvette Temp
Casting Temperature 2000 - 2200 °C
 
Component Elements PropertiesOriginal ValueComments
Iridium, Ir 10 %
Platinum, Pt 90 %
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wieland 1757 Wilaform Platinum
Overview of materials for Platinum Alloy
Johnson Matthey SW 900 Platinum w/ 10% Iridium Jewelry Alloy
Goodfellow Platinum 90/Iridium 10 Alloy

NWIELAN81 / 19883

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.