MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® 996/M55J Siloxane Resin/Fabric
Categories: Polymer; Thermoplastic; Siloxane

Material Notes:

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 5.70 ksi
@Temperature 82.2 °C
90º Tension, wet; ASTM 3039
 5.80 ksi
@Temperature -55.0 °C
90º Tension, dry; ASTM 3039
 6.10 ksi
@Temperature 22.8 °C
90º Tension, dry; ASTM 3039
 270 ksi
@Temperature 82.2 °C
0º Tension, wet; ASTM 3039
 286 ksi
@Temperature 22.8 °C
0º Tension, dry; ASTM 3039
 289 ksi
@Temperature -55.0 °C
0º Tension, dry; ASTM 3039
Tensile Modulus 45950 ksi
@Temperature 22.8 °C
0º Tension, dry; ASTM 3039
 46390 ksi
@Temperature 82.2 °C
0º Tension, wet; ASTM 3039
 46670 ksi
@Temperature -55.0 °C
0º Tension, dry; ASTM 3039
Compressive Strength 11.4 ksi
@Temperature 82.2 °C
0º, wet; SACMA SRM-1R94
 129.1 ksi
@Temperature 22.8 °C
0º, dry; SACMA SRM-1R94
 136.3 ksi
@Temperature -55.0 °C
0º, dry; SACMA SRM-1R94
Compressive Modulus 45880 ksi
@Temperature -55.0 °C
0º, dry; SACMA SRM-1R94
 48000 ksi
@Temperature 82.2 °C
0º, wet; SACMA SRM-1R94
 49460 ksi
@Temperature 22.8 °C
0º, dry; SACMA SRM-1R94
Shear Modulus 620 ksiIn-Plane; SMR-7R94
Shear Strength 10.9 ksiIn-Plane; SMR-7R94
 7.80 ksi
@Temperature 82.2 °C
Short Beam, 0º, dry; ASTM 2344
 10.7 ksi
@Temperature -4.44 °C
Short Beam, 0º, dry; ASTM 2344
 12.6 ksi
@Temperature -55.0 °C
Short Beam, 0º, dry; ASTM 2344
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.45
@Frequency 9.375e+6 Hz,
Temperature 121 °C
 5.54
@Frequency 9.375e+6 Hz,
Temperature 23.9 °C
Dielectric Loss Index 0.00800
@Frequency 9.375e+6 Hz,
Temperature 23.9 °C
 0.0120
@Frequency 9.375e+6 Hz,
Temperature 121 °C
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 160.4 °C
@Temperature 82.2 °C
RDS Torsion, G1; T-41
 169.6 °C
@Temperature 23.9 °C
RDS Torsion, G1; T-41

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHEXCB9112 / 322268

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.