MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Quantum Composites QC-8151C 55% Glass Fiber Vinyl Ester Static-Dissipative SMC  (discontinued **)
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Vinyl Ester; Vinyl Ester Sheet Molding Compound

Material Notes: QC-8151C is a vinyl ester sheet molding compound (SMC) designed for compression molding components requiring dimensional stability, resistance to high temperatures plus sufficient electrical conductivity to dissipate static charge. It also offers excellent chemical resistance, light weight, low heat absorption and high strength at both room and elevated temperatures. This electrical conductivity is built into and throughout the composite. It is designed to mold and cure at lower temperatures than QC-8150C. Form and Color = Rolled Sheet, Gray. Glass Fiber Length = 1 inch.

A. Schulman has acquired Quantum Composites.

Key Words: Sheet Molding Compound
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.75 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 206 MPaASTM D638
Flexural Yield Strength 344 MPaASTM D790
Flexural Modulus 15.1 GPaASTM D790
Izod Impact, Notched 12.8 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Shrinkage 0.00020 %
 
Processing PropertiesOriginal ValueComments
Processing Temperature 93.0 - 121 °CMold temperature

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Quantum Composites QC-8100 60% Glass Fiber Vinyl Ester SMC
Quantum Composites QC-8704 63% Glass Fiber Vinyl Ester SMC
Quantum Composites QC-8800 63% Glass Fiber Vinyl Ester SMC
Quantum Composites QC-8805 66% Glass Fiber Vinyl Ester SMC
A. Schulman BMC 845 Vinyl Ester Molding Compounds, 30% Glass-Filled

PCOQC7 / 29044

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.