MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Esenttia 01R25-T Random Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Characteristics: Natural color highly heat stabilized high molecular weight fractional melt flow rate Random copolymer polypropylene; formulated for extraction resistance; consistent processability; good transparency; high cleanness; good resistance to chemicals and surfactants.

Recommended for: Pipe extrusion and injection molding of Fittings for hot and cool water process, offering exceptional hydrostatic strength combined with excellent chemical resistance and weldability; tanks and pipes for the chemical industry; extrusion blow molding containers.

Information provided by Esenttia by Propilco

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 0.26 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238B
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 25.51 MPa50 mm/min; ASTM D638
Elongation at Yield 14 %50 mm/min; ASTM D638
Flexural Modulus, 1% Secant 813.6 MPa1.3 mm/min; ASTM D790-1A
Izod Impact, Notched 533.79 J/mASTM D256-A
Gardner Impact 29.38 JASTM D5420A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Formosa Plastics Formolene® 4100N Injection Molding Polypropylene
Total PPC 1640 Polypropylene, Heterophasic Copolymer, Non-pressure Pipes
Dow H103-00 Polypropylene Homopolymer
Esenttia 03H82 Homopolymer Polypropylene
Formosa Plastics Formolene® 4100P Injection Molding Polypropylene

PESEN029 / 184601

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.