MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow DT702 TPO
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Dow Fascia TPO for Painted Applications

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.901 g/ccASTM D792
Linear Mold Shrinkage 0.0044 - 0.0048 cm/cmUnannealed; ASTM D955
 0.0050 - 0.0055 cm/cmAnnealed; ASTM D955
Melt Flow 13.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 2340 psiASTM D638
Tensile Strength, Yield 2950 psiASTM D638
Elongation at Break 564 %ASTM D638
Elongation at Yield 5.6 %ASTM D638
Tensile Modulus 151000 psiASTM D638
Flexural Modulus 148000 psiASTM D790A
Izod Impact, Notched 2.30 ft-lb/in0°F; ASTM D256A
 3.50 ft-lb/in32°F; ASTM D256A
 11.0 ft-lb/in72°F; ASTM D256A
Instrumented Impact Energy at Peak 161 in-lbID Impact @ 5mph, Peak Energy; ASTM D3763-86
 280 in-lbID Impact @ 5mph, Total Energy; ASTM D3763-86

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow TF0807 TPO
Dow INSPIRE™ DT701-14 TPO
Borealis Daplen™ VB4411 TPO Compound
Borealis Daplen™ ED206HP TPO Compound
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)

PDOW1134 / 30338

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.