MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Precision Polymer Engineering R70D Natural Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Natural Rubber, 65-75 °IRHD. Formulated to Defence Standard 93-30, Type QX, Grade 70 (NRQX70).

Applications: Natural rubber offers low compression set, high tensile strength, high resilience and excellent resistance to tear and abrasion. The designation `Type QX` indicates that the material is suitable for certain applications where a high degree of compatibility with explosives is a requirement. However, compatibility with all explosives in all environments has not been established and design authorities should seek advice on particular applications from the Director, Defence Research Agency (Military Division), Fort Halstead, Sevenoaks, Kent, TN14 7BP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70°IRHD; ASTM D1415
 70 - 74°IRHD, -0/+4 change after 168 hours @ 70°C; ASTM D1415
Tensile Strength, Yield 10.2 MPa-15% change after 168 hours @ 70°C; ASTM D412
 12.0 MPaASTM D412
Elongation at Break 255 %-15% change after 168 hours @ 70°C; ASTM D412
 300 %ASTM D412
Compression Set 35 %
@Temperature 70.0 °C,
Time 86400 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 100 °C
Minimum Service Temperature, Air -50.0 °C
Flash Point >= 300 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Precision Polymer Engineering R80Z Natural Rubber
Precision Polymer Engineering R70Z Natural Rubber
Precision Polymer Engineering R60R Natural Rubber
Precision Polymer Engineering R60D Natural Rubber
Precision Polymer Engineering R50Z Natural Rubber

PPRECI170 / 57894

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.