MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Taiwan PU SHB303020 PU Sheet
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Key features:
  • High tensile strength and elasticity
  • Good abrasion-resistant
  • Excellent impact resistance
  • Wide hardness range
  • Tough, crack-resistant
Application: PU Sheet can use for sports equipment, building materials, petroleum, mining, automobile. For example, cushioning pads, block, springs, metal plates, pipes and die materials of heavy machinery and stamping equipments . You can use its friction, vibration reduction and buffer in the mechanical equipments.

Information provided by Taiwan PU Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9393
Tensile Strength 37.75 MPa5475 psi
Elongation at Break 431 %431 %
100% Modulus 9.18 MPa1330 psi
300% Modulus 16.4 MPa2380 psi
Rebound 42 %42 %Bashore
Tear Strength 21.9 kN/m125 pliDie C; ASTM D1938
 51.4 kN/m293 pliDie C; ASTM D624
Compression Set 32 %
@Temperature 21.1 °C,
Time 79200 sec
32 %
@Temperature 70.0 °F,
Time 22.0 hour
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature >= 62.0 °C>= 144 °FBell

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTAIWPU449 / 306179

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.