MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Pyrotek Pyrocast SC-2600 Castable Refractory
Categories: Ceramic; Carbide

Material Notes: Pyrocast SC-2600 is a high purity silicon carbide based refractory for applications requiring high thermal conductivity, resistance to metal and flame abrasion.

Applications

  • Filter boxes
  • Burner tubes
  • Troughs
  • Tap out blocks
  • Special refractory shapes
  • Baffles
  • Filter bowl tiles

Advantages

  • Resistant to metal
  • Resistant to flame abrasion
  • High thermal conductivity
  • Withstands high temperatures
  • Extremely hard

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.40 g/cc
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00800 GPa
@Temperature 90.0 °C
 0.0220 GPa
@Temperature 815 °C
 0.0300 GPa
@Temperature 1370 °C
Compressive Strength 10.0 MPa
@Temperature 815 °C
 19.0 MPa
@Temperature 90.0 °C
 19.0 MPa
@Temperature 1370 °C
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 9.40 - 10.8 W/m-K
Maximum Service Temperature, Air 1480 °C
Shrinkage -0.600 %
@Temperature 1300 °C
Linear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pyrotek Pyrocast AR70 Low-Density Refractory Castable
Pyrotek Pyrocast HD Castable Refractory
Pyrotek Pyrocast L-40 Insulating Refractory
Pyrotek Pyrocast 80 Lightweight Castable Refractory
Pyrotek Pyrocast AR-S Castable Refractory

CPYRO083 / 1821

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.