FM 1216 is a halogen free bedding compound for cable and wire with maximum 90ºC operating temperature at conductor and Insulation: 2 XI 1 XLPE (acc. DIN/VDE 0207 Part 22) or 2 YI 1-5 PE (acc. DIN/VDE 0207 Part 2); and Sheathing: 2 YM 3 HDPE (acc. DIN/VDE 0207 Part 3); and other standards. Non-flame retardant; XLPE, PE Insulation: PE Sheathing Applications: Market: PolyOne First ChoiceInformation provided by PolyOne Corporation. |