MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Marco Polo MARPOL PSH 6132 HIPS
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Description: MARPOL ® PSH 6132 is a high melt flow, high impact polystyrene specially designed for hard to fill injection molding applications. It is ideal for large parts, thin wall parts or molds with complex runner and gate systems.

Recommended Applications: Thin wall injection molding, textile spools and medical applications

This material complies with FDA requirements as described in 21 CFR 177.1640.

Information provided by Marco Polo International, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/cc
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmASTM D955
Melt Flow 13 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 3300 psiASTM D638
Tensile Modulus 2210 MPaASTM D638
Flexural Strength 5700 psiASTM D790
Flexural Modulus 300000 psiASTM D790
Izod Impact, Notched 2.10 ft-lb/inASTM D256
Falling Dart Impact 10.0 ft-lbASTM D 3029
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 93.3 °CASTM D1525
Heat Distortion Temperature 189 °FAnnealed; ASTM D648
 
Optical PropertiesOriginal ValueComments
Gloss 94 %60°; ASTM D253
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMARCO230 / 283827

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.