MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Thermoseal

Klinger Thermoseal soft-chem® PTFE Gasketing
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Thermoseal® soft-chem® expanded PTFE sealing material provides excellent corrosion resistance and impermeability along with superior creep resistance and sealability for use in all types of applications. The material's high compressibility enables it to deform under load and conform to irregularities in flange faces for a tight seal with low, minimum sealing stress. Standardizing with it also helps to reduce maintenance, simplify inventory, and save money.
  • Can be used with more fragile piping systems
  • Ideal for boiler applications because it's largely unaffected by steam or condensate for longer life and trouble-free sealing
  • BAM approval for gaseous oxygen
  • Indefinite self life
  • FDA compliant

Information provided by Thermoseal Inc.

Vendors: Thermoseal Inc. is the exclusive North American producer of Klinger Fluid Sealing products, including popular lines: Sealex, Klingersil and Topchem and our new Performance Technology Group of products. Visit us at Thermosealinc.com or call 1-800-990-7325 to speak with a fluid sealing specialist.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.850 g/cc0.0307 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 10.3 MPa1500 psiASTM D152
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
Chemical Resistance0-14 pH
Compressibility60 percentASTM F36
Creep Relaxation35 percent1/32", ASTM F38B
Gas Permeability0.12 ml/hrDIN 3535/6
Gasket Constants0.2 psia, 1/16", tested by Ecole Polytechnic
 1260 psiGb, 1/16", tested by Ecole Polytechnic
 3.5 psiGs, 1/16", tested by Ecole Polytechnic
Klinger Hot Compression Test28.6 percentThickness Decrease Hot, 572°F (300°C)
 37 percentThickness Decrease Ambient, 3625 psi
Recovery>12 percentASTM F36
Sealability.002 ml/minASTM F37 B Fuel A
Vacuum to Full Pressure3000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1045 Steel, turned, ground, and polished, 19-32 mm (0.75-1.25 in) round
AISI 1045 Steel, Quenched and Tempered to 595 HB
AISI 1018 Steel, cold drawn, high temperature, stress relieved, 22-32 mm (0.875-1.25 in) round
AISI 1018 Steel, as cold drawn, 32-50 mm (1.25-2 in) round
Mitsui APEL™ APL5014DP Cyclo Olefin Copolymer (COC)

PTHERM924 / 146078

Thermoseal

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.