MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Celanex® 1462Z PBT, 30% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Celanex 1462Z is a general purpose, 30% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.52 g/ccASTM D792
Density 1.52 g/ccISO 1183
Water Absorption 0.050 %
@Temperature 22.8 °C
24hr immersion; ASTM D570
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cmISO 294-4
 0.0030 - 0.0050 cm/cmASTM D955
Melt Flow 14 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 90ISO 2039-2
Tensile Strength at Break 135 MPa5mm/min; ISO 527-2/1A
 18000 psiASTM D638
Elongation at Break 2.6 %5mm/min; ISO 527-2/1A
 4.0 %ASTM D638
Flexural Strength 210 MPaISO 178
 28500 psiASTM D790
Flexural Modulus 9110 MPaISO 178
 1.20e+6 psiASTM D790
Izod Impact, Notched 1.70 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 9.20 kJ/m²ISO 180/1A
Charpy Impact, Notched 7.20 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Strength 520 V/milshort term; ASTM D149
Dissipation Factor 0.0020
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 25.0 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 128 µm/m-°CISO 11359-2
Melting Point 225 °C10°C/min; ISO 11357-1,-2,-3
 437 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 225 °CISO 75-1, -2
 422 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 207 °CISO 75-1, -2
 400 °FASTM D648
Glass Transition Temp, Tg 60.0 °CISO 11357-1,-2,-3
Flammability, UL94 HB
 HB
@Thickness 0.800 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 65.0 - 93.0 °Ccavity
 250 - 260 °Chot runner
Feed Temperature 230 - 240 °C
Zone 1 230 - 240 °C
Zone 2 235 - 250 °C
Zone 3 235 - 250 °C
Zone 4 240 - 260 °C
Die Temperature 250 - 260 °C
Melt Temperature 235 - 260 °C
 260 °CISO 294
Mold Temperature 82.0 °CISO 294
Injection Velocity 300 mm/secISO 294
Drying Temperature 120 - 130 °C
Dry Time 4.00 hour
Moisture Content <= 0.020 %
Hold Pressure 48.0 MPaISO 294
 
Descriptive Properties
Injection moldingYes
Injection speedmedium-fast
Processing conditions acc. ISO7792-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Celanex® 1602Z PBT, Unfilled
Celanese Celanex® 2401 MT PBT, Medical Technology
Celanese Celanex® 2402 MT PBT, Medical Technology
Clariant Renol PBT1700G30BK Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant
Clariant Renol PBTG30-L Polybutylene Terephthalate, 30% Glass Reinforced

PHCQ003 / 178458

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.