An expandable, low gravity, injection molding compound specifically developed for footwear applications. Finished product appearance is matte, similar to TPR. Information provided by Georgia Gulf Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued. |