MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis BE52 Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Blow Molding Grade

Material Notes: BE52 is a polypropylene homopolymer intended for blow molding and thermoforming. The product is available in natural color. This material has excellent balanced mechanical properties and is easy to process.

Applications: BE52 is intended for following applications:

  • Washing machine parts
  • Dishwashers components
Typical characteristics: BE52 can be described with following typical characteristics:
  • High heat stabilized
  • UL94 listed

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO 1183-1/Method A
Melt Flow 0.250 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
Storage Temperature <= 50.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 35.0 MPa50 mm/min; ISO 527-2
Flexural Modulus 1300 MPaISO 178
Charpy Impact, Notched 8.00 kJ/m²ISO 179-1/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °CISO 75-2
Shrinkage 2.00 %Average
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 230 °CCylinder
 190 - 230 °CBarrel
Die Temperature 190 - 230 °C
Melt Temperature 190 - 230 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9609 / 322966

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.