MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Petrothene GA623119 Linear Low Density Polyethylene (LLDPE)/Hexene, Molded
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Extrusion Grade; LLDPE/Octene, Extruded; LLDPE/Hexene, Molded

Material Notes: Petrothene GA623119 is a hexene LLDPE copolymer selected for applications that require high clarity and good stiffness combined with low COF. GA623119 is formulated without TNPP, slip or antiblock additives. Applications: Bags & Pouches, Can Liners, Clarity Film, Film Wrap, Food Packaging Film, Lamination Film, Liner Film, Zipper Packaging

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.923 g/ccASTM D1505
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 740 %ASTM D882
Film Elongation at Break, TD 840 %ASTM D882
Elmendorf Tear Strength MD 540 gASTM D1922
Elmendorf Tear Strength TD 890 gASTM D1922
Dart Drop Test 200 gF50; ASTM D1709
Film Tensile Strength at Break, MD 37.2 MPaASTM D638
Film Tensile Strength at Break, TD 40.0 MPaASTM D638
1% Secant Modulus, MD 252 MPaASTM D882
1% Secant Modulus, TD 285 MPaASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 5.4 %ASTM D1003
Gloss 85 %ASTM D2457
 
Descriptive Properties
Processing MethodBlown Film, Cast Film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Petrothene GA574200 Linear Low Density Polyethylene (LLDPE), Injection Molded
LyondellBasell Petrothene GA578189 Linear Low Density Polyethylene (LLDPE), Injection Molded
Dow DOWLEX™ 2267G Linear Low Density Polyethylene
Dow DNDA-9810 NT 7 Linear Low Density Polyethylene Resin
Dow ASPUN™ 6830A Linear Low-Density Polyethylene (LLDPE)

PEQT8826 / 220460

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.