MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical EM600A Impact modifier for Engineering Plastics  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: LG Chem impact modifiers for Engineering Plastics are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modifiers - Butadiene type, Acryl type.

Application: PMMA, PC Alloy (PC, PC/ABS, PC/PBT) etc

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/cc
Bulk Density >= 0.360 g/ccAerated; LSY-QB-KD019
Volatiles <= 1.0 %ISO 1625
Particle Mesh Size 10 Mesh<5%, (mesh on); LSY-QB-KD038
 200 Mesh<20%, (mesh pass); LSY-QB-KD039
 
Mechanical PropertiesOriginal ValueComments
Izod Impact, Unnotched >= 3.00 kg-cm/cm
@Temperature 23.0 °C
ISO 180
 
Thermal PropertiesOriginal ValueComments
Melting Point 132 - 149 °C
 
Optical PropertiesOriginal ValueComments
Haze <= 2.0 %LSY-QB-KD014
 
Descriptive Properties
Foreign Material<3 (10 x 10 cm)LSY-QB-KD005

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Oceanchem Group Melamine Polyphosphate (MPP)
LG Chemical EM500 Impact modifier for Engineering Plastics
LG Chemical EM500A Impact modifier for Engineering Plastics
Arkema LOTADER® AX 8900 Terpolymer Ethylene - Acrylic Ester - Glycidyl Methacrylate
LG Chemical EM600 Impact modifier for Engineering Plastics

PLAY634 / 148644

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.