MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trelleborg AEM Eccospheres® SI-250 Sodium Borosilicate Glass Microspheres
Categories: Ceramic; Glass; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnification reveals them to be near perfect spheres.

    Properties
  • High temperature resistance
  • Good density/strength ratios
  • Clean surface chemistry
  • Narrow particle size distribution
  • Low thermal conductivity
  • Low dielectric constant
  • Low dissipation factor

Surface salts formed during manufacture are removed via acid washing. This reduces the alkali content and results in a clean surface chemistry compatible with almost any resin system or surface coating.

All information provided by Trelleborg Emerson & Cuming

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Pellet Density 0.230 - 0.270 g/ccASTM D2840
Particle Size 52 µmTEC QSD
pH 6.5 - 9.0ASTM D4876
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 62.0 GPa
@Temperature 25.0 °C
 62.0 GPa
@Temperature 25.0 °C
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 1.36 - 1.63
@Frequency 1e+8 Hz
ASTM D150
Dissipation Factor 0.00050
@Frequency 1e+6 - 8.60e+9 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0730 - 0.125 W/m-K
Softening Point 800 °CASTM E794
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.448
@Wavelength 1500 nm
 1.458
@Wavelength 589.3 nm
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 1.0 %TED QSD
 
Descriptive Properties
Floatation (% bulk volume)99TEC QSD
Isostatic Collapse Pressure, Min. 80% Survival (psi)1800ASTM D3102
Packing Factor (min)62

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trelleborg AEM Eccospheres® SI-200 Sodium Borosilicate Glass Microspheres
Trelleborg AEM Eccospheres® SI-350 Sodium Borosilicate Glass Microspheres
Trelleborg AEM Eccospheres® W-25 Sodium Borosilicate Glass Microspheres
Trelleborg AEM Eccospheres® IG-101 Sodium Borosilicate Glass Microspheres
3M K37 Glass Bubbles

PTRELL188 / 83946

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.