MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

(Viewing data as-entered. Click here to return)
Trimay® Wear Plate TWP170 Flux Cored Weld Wire & Electrode
Categories: Metal; Nonferrous Metal; Nickel Alloy; Tungsten Alloy

Material Notes: Wire Description: TWP70 is a flux cored wire electrode for open-arc welding. Macrocrystalline tungsten carbide, nickel and boron fill a pure nickel tube which can be welded with or without shielding gas. Macrocrystalline tungsten has a higher melting point than that of the molten welding puddle, therefore the matrix is not affected by the degradation of Tunsten carbides throughout the matrix. The result is a stable matrix which is not brittle and can absorb impact without cracking.

Key Performance Characteristics: Highest abrasion resistance, Highest impact resistance, Uniform carbide distribution throughout weld deposit, Crackless weld deposit

Applications:TWP70 can be applied on ferritic and austenitic steels using a open or closed arc welding procedure, with or without gas shielding. TWP70 is used to overlay and protect areas which are exposed to the most extreme abrasion and/or impact. TWP70 has been used for diamond bit augers, cement factory fan blades, bucket teeth, and crusher rolls.

Information provided by Trimay®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 48 - 50Electrodes
 50 - 55Wire
 
Component Elements PropertiesOriginal ValueComments
Boron, B <= 5.0 %
Nickel, Ni 30 - 50 %
WC 48 - 62 %macrocrystalline
 
Descriptive Properties
Available Sizes: Electrode5[mm]
 6.4[mm]
Available Sizes: Wire1.6[mm], cored wire
 2.4[mm], cored wire
 2.8[mm], cored wire
Packaging: Electrode1All Sizes- 5kg sleeves
Packaging: Wire1All Sizes- 25kg coils

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for High Carbon Steel
Overview of materials for Chrome-moly Steel
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M77HS Moldable
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M33 Moldable
Mid-Mountain Materials THERMOSEAL® 2000 High Temperature Cement

NTRIM009 / 120823

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.