MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Copper, UNS C15500, Quarter Hard
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability; good forgeability. Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping.

Applications: high conductivity light-duty springs, electrical contacts, fittings, clamps, connectors, diaphragms, electronic components, resistance welding electrodes.

Available as flat products, 5mm thick. 8.30 oz/ton Ag.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.90 g/cc0.322 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell F 8989
Tensile Strength, Ultimate 310 MPa45000 psi
Tensile Strength, Yield  246 MPa
@Strain 0.2 %
35700 psi
@Strain 0.2 %
 248 MPa
@Strain 0.5 %
36000 psi
@Strain 0.5 %
Elongation at Break 28 %28 %In 50 mm
Modulus of Elasticity 115 GPa16700 ksi
Poissons Ratio 0.3070.307
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 44.0 GPa6380 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000192 ohm-cm
@Temperature 20.0 °C
0.00000192 ohm-cm
@Temperature 68.0 °F
annealed condition after precipitation heat treatment
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.7 µm/m-°C
@Temperature 20.0 - 300 °C
9.83 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.385 J/g-°C0.0920 BTU/lb-°F
Thermal Conductivity 345 W/m-K2390 BTU-in/hr-ft²-°F
Melting Point 1078 - 1080 °C1972 - 1980 °F
Solidus 1078 °C1972 °F
Liquidus 1080 °C1980 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 485 - 540 °C905 - 1000 °F
Hot-Working Temperature 750 - 875 °C1380 - 1610 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 99.75 %99.75 %
Magnesium, Mg 0.080 - 0.13 %0.080 - 0.13 %
Phosphorus, P 0.040 - 0.080 %0.040 - 0.080 %
Silver, Ag 0.027 - 0.10 %0.027 - 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper, UNS C15500, O50 (Light Anneal) Temper
Oxygen-free high conductivity Copper, Hard, UNS C10200
Chromium Copper, UNS C18500
Chromium Copper, UNS C18400
Chromium Copper, UNS C18200, TB00 Temper flat products

MC15500c2 / 10665

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.