MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hostacom HYG 400-2 BLACK Polypropylene with 20% Glass Fiber Filler
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Glass Fiber Filler

Material Notes: Hostacom HYG 400-2 BLACK is a 20% glass fiber reinforced PP homopolymer, with very high flowability, low emissions and high stiffness. The product is available in black color, pellet form. Applications: Automotive Parts

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183-1
Melt Flow 63 g/10 min
@Load 2.16 kg,
Temperature 230 °C
63 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 115 MPa16700 psiISO 2039-1
Tensile Strength, Yield 80.0 MPa11600 psiISO 527-1,-2
Elongation at Break 3.0 %3.0 %ISO 527-1,-2
Tensile Modulus 4.80 GPa696 ksiISO 527-1,-2
Charpy Impact Unnotched 4.00 J/cm²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eU
Charpy Impact, Notched  0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1/1eA
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 135 °C275 °Funannealed; ISO 75A-1,-2
Vicat Softening Point 128 °C262 °FB50; ISO 306
 
Descriptive Properties
Ball Indentation Hardness (MPa)358N
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polykemi AB POLYfill PPC TS16020 LE Polypropylene Copolymer, Mineral Reinforced, Low Emission
Polyplastic Armlen® PP MF 20-3-901 Polypropylene, 20% Mineral Filled
LyondellBasell Hostacom TRC 333N D22713 Polypropylene with 20% Talc Filler
LyondellBasell Hostacom TRC 333N C12334 Polypropylene with 20% Talc Filler
LyondellBasell Hostacom TRC 333N C1 NATURAL Polypropylene with 20% Talc Filler

PEQT8000 / 219636

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.