MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Lupranate® 265 Isocyanate
Categories: Fluid

Material Notes: Description: Lupranate® 265 Isocyanate, a solid at room temperature, is essentially pure 4,4´-diphenylmethane diisocyanate, having a functionality of 2.0. Lupranate 265 Isocyanate is used in the isocyanate component for the preparation of elastomeric and thermoplastic polyurethanes, flexible and semi-flexible integral skin foams, adhesives, sealants and coatings. Lupranate 265 Isocyanate is BHT-free and contains a phosphite stabilizer in its place.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/cc
Vapor Pressure 4.00e-7 bar
@Temperature 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Melting Point 38.5 °C
Boiling Point >= 190 °C
@Pressure 0.000667 MPa
Flash Point 199 °C
 
Descriptive Properties
ColorWhite to Light Yellow
Composition2,4' Isomer0.02
 Hydrolyzable Chlorine<20 ppm
 NCO content0.335
Purity99.5 percent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Lupranate® 219 Isocyanate Modified MDI
BASF Lupranate® MS Isocyanate
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
BASF Lupranate® 227 Isocyanate
BASF Lupranate® 245 Isocyanate

PBASG0658 / 132291

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.