MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Greene Tweed CHEMRAZ® 571 Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Chemraz® 571 is recommended for a wide variety of semiconductor equipment wet processing applications where stringent seal reliability and contamination control are required. This seal material offers excellent performance in ling-term static sealing applications in acid, solvent and ultra pure H2O. Chemraz 571 is excellent for high sealing load designs.

Applications:

  • Valve seals
  • Fitting and union seals
  • Gasket seals
  • Regulator seals
  • Filter seals
  • Dispensing seals

Information provided by Greene Tweed.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.99 g/ccASTM D297
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80ASTM D2240
Tensile Strength at Break 1550 psiASTM D1414
Tensile Strength, Yield 625 psi@50% Elongation; ASTM D1414
 1240 psi@100% Elongation; ASTM D1414
Elongation at Break 130 %ASTM D1414
Compression Set 35 %
@Temperature 204 °C,
Time 252000 sec
At 25% deflection; ASTM D395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 410 °F
Minimum Service Temperature, Air -22.0 °F
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Greene Tweed CHEMRAZ® 585 Perfluoroelastomer
Greene Tweed CHEMRAZ® 592 Perfluoroelastomer
Greene Tweed CHEMRAZ® 584 Perfluoroelastomer
Greene Tweed CHEMRAZ® 570 Perfluoroelastomer
Greene Tweed CHEMRAZ® 565 Perfluoroelastomer

PGREEN18 / 42312

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.