MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Ixef® 3008 Polyarylamide (PARA), 30% carbon fiber
Categories: Polymer; Thermoplastic; Polyarylamide (PAA)

Material Notes: Ixef® 3008 is a 30% carbon-fiber reinforced polyarylamide compound which exhibits extremely high strength and stiffness, good surface gloss, excellent creep resistance, and lower density than glass-fiber reinforced engineering resins.

Black: Ixef® 3008/9008

Markets/Uses: Automotive / Mechanical & Structural Parts / Accumulator Piston; Automotive / Mechanical & Structural Parts / Air Intake/Lamella; Automotive / Mechanical & Structural Parts / Body Components; Automotive / Mechanical & Structural Parts / Brackets; Automotive / Mechanical & Structural Parts / Brake Power Pistons; Automotive / Mechanical & Structural Parts / Bushings; Automotive / Mechanical & Structural Parts / Center Drive Assembly; Automotive / Mechanical & Structural Parts / Clutch Cylinder; Automotive / Mechanical & Structural Parts / Door Handles; Automotive / Mechanical & Structural Parts / Door Lock Components; Automotive / Mechanical & Structural Parts / Electric Gas Pedal Support; Automotive / Mechanical & Structural Parts / Engine Mount Orifice; Automotive / Mechanical & Structural Parts / Gears; Automotive / Mechanical & Structural Parts / Poppets; Automotive / Mechanical & Structural Parts / Side Mirror Support; Automotive / Mechanical & Structural Parts / Sunroof Structural Components; Electronics / Mobile Devices Electronic Components / Microspeakers; Electronics / Mobile Devices Electronic Components / Microswitches; Electronics / Mobile Devices Structural / Battery Covers; Electronics / Mobile Devices Structural / Camera Modules; Electronics / Mobile Devices Structural / Chassis and Frames

Applications: Appliance Components; Appliances; Automotive Applications; Automotive Electronics; Automotive Under the Hood; Bushings; Camera Applications; Cams; Cell Phones; Electrical/Electronic Applications; Furniture; Gears; Industrial Applications; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal Replacement; Power/Other Tools

Features: Chemical Resistant; Creep Resistant; Good Dimensional Stability; High Flow; High Strength; Low Moisture Absorption; Outstanding Surface Finish; Ultra High Stiffness

Injection notes: Hot Runners: 250°C to 260°C (482°F to 500°F)
Injection Pressure: rapid
Storage
Ixef® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Ixef® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Ixef® processing guide.
Drying
The material as supplied is ready for molding without drying. However, If the bags have been open for longer than 24 hours, the material needs to be dried. When using a desiccant air dryer with dew point of -28°C (-18°F) or lower, these guidelines can be followed: 0.5-1.5 hour at 120°C (248°F), 1-3 hours at 100°C (212°F), or 1-7 hours at 80°C (176°F).
Injection Molding
IXEF 3008 compound can be readily injection molded in most screw injection molding machines. A general purpose screw is recommended, with minimum back pressure.
The measured melt temperature should be about 280°C (536°F), and the barrel temperatures should be around 250°C to 260°C (482°F to 500°F) in the rear zone, gradually increasing to 260°C to 280°C (500°F to 536°F) in the front zone. If hot runners are used, they should be set to 250°C to 260°C (482°F to 500°F).
To maximize crystallinity, the temperature of the mold cavity surface must be held between 120°C and 140°C (248°F and 284°F). Molding at lower temperatures will produce articles that may warp, have poor surface appearance, and have a greater tendency to creep. Set injection pressure to give rapid injection. Adjust holding pressure and hold time to maximize part weight. Transfer from injection to hold pressure at the screw position just before the part is completely filled (95%-99%).

Information provided by Solvay Specialty Polymers.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.34 g/ccISO 1183
Water Absorption 0.22 %
@Time 86400 sec
ISO 62
Moisture Absorption at Equilibrium 2.0 %65% RH; ASTM D570
Linear Mold Shrinkage, Flow 0.00030 - 0.0010 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 250 MPaISO 527-2
Elongation at Break 1.3 %ISO 527-2
Tensile Modulus 26000 MPaISO 527-2
Flexural Strength 360 MPaISO 178
Flexural Modulus 23000 MPaISO 178
Izod Impact, Notched 59.0 J/mASTM D256
Izod Impact, Unnotched 450 J/mASTM D256
Charpy Impact Unnotched 36.0 kJ/m²ISO 179
Charpy Impact, Notched 3.60 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3000 ohm-cmASTM D257
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 230 °CUnannealed; ISO 75-2/A
Flammability, UL94 HB
Oxygen Index 23 %ISO 4589-2
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 250 - 260 °C
Front Barrel Temperature 260 - 290 °C
Melt Temperature 280 °CInjection
Mold Temperature 120 - 140 °C
Drying Temperature 120 °C
@Time 1800 - 5400 sec
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets
ProcessingInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4282 / 280082

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.