MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Radici RADILON® S RV500K 333 BK Nylon 6, 50% Glass Fiber Reinforced, Heat Stabilized, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 50% Glass Fiber Filled; Nylon 6, Heat Stabilized

Material Notes: Description: PA6 50% glass fiber reinforced injection molding grade. Heat stabilized. Black color. Suitable for parts requiring very high stiffness and high mechanical resistance, as in case of metal replacement applications. Good resistance to thermal ageing.

Processing: Injection Molding

Delivery Form: Granules

Additives: Release agent

Special Characteristics: Heat stabilized or stable to heat, DPPD Free

Industries: Automotive, Consumer Industry Goods, Transportation

Regional Availability: North America, Europe, Asia Pacific, South and Central America, Near East/Africa

Information provided by Radici Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.57 g/ccISO 1183
Water Absorption 4.8 %
@Thickness 2.00 mm
Immersion at 23°C; ISO 62
Moisture Absorption 1.40 %
@Thickness 2.00 mm
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cmMelt Temp/Mold Temp/Cavity Pressure: 280/90/60; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cmMelt Temp/Mold Temp/Cavity Pressure: 280/90/60; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 215 MPa5mm/min; ISO 527-2/1A
Tensile Stress 45.0 MPa
@Strain 2 %,
Temperature 160 °C
Break
 55.0 MPa
@Strain 4 %,
Temperature 160 °C
Break
 80.0 MPa
@Strain 2 %,
Temperature 120 °C
Break
 95.0 MPa
@Strain 4 %,
Temperature 120 °C
Break
 100 MPa
@Strain 0.9 %,
Temperature 80.0 °C
Break
 100 MPa
@Strain 0.8 %,
Temperature 40.0 °C
Break
 100 MPa
@Strain 1.1 %,
Temperature 60.0 °C
Break
 100 MPa
@Strain 0.75 %,
Temperature 23.0 °C
Break
 125 MPa
@Strain 4 %,
Temperature 80.0 °C
Break
 150 MPa
@Strain 4 %,
Temperature 60.0 °C
Break
 180 MPa
@Strain 2 %,
Temperature 40.0 °C
Break
 200 MPa
@Strain 1.8 %,
Temperature 23.0 °C
Break
Elongation at Break 2.7 %5mm/min; ISO 527-2/1A
Tensile Modulus 16500 MPa1mm/min; ISO 527-2/1A
Flexural Strength 335 MPa2mm/min; ISO 178
Flexural Modulus 14500 MPa2mm/min; ISO 178
Secant Modulus 1.50 GPa
@Strain 4 %,
Temperature 160 °C
Break
 2.00 GPa
@Strain 2 %,
Temperature 160 °C
Break
 2.50 GPa
@Strain 4 %,
Temperature 120 °C
Break
 3.50 GPa
@Strain 4 %,
Temperature 80.0 °C
Break
 4.00 GPa
@Strain 0.3 %,
Temperature 160 °C
Break
 4.00 GPa
@Strain 2 %,
Temperature 120 °C
Break
 5.00 GPa
@Strain 3 %,
Temperature 60.0 °C
Break
 5.00 GPa
@Strain 2 %,
Temperature 80.0 °C
Break
 6.50 GPa
@Strain 3 %,
Temperature 40.0 °C
Break
 7.00 GPa
@Strain 0.1 %,
Temperature 120 °C
Break
 10.0 GPa
@Strain 0.75 %,
Temperature 60.0 °C
Break
 10.0 GPa
@Strain 1.7 %,
Temperature 40.0 °C
Break
 10.1 GPa
@Strain 2 %,
Temperature 23.0 °C
Break
 12.0 GPa
@Strain 0.1 %,
Temperature 80.0 °C
Break
 17.5 GPa
@Strain 0.0 %,
Temperature 60.0 °C
Break
 17.5 GPa
@Strain 0.0 %,
Temperature 23.0 °C
Break
 19.0 GPa
@Strain 0.0 %,
Temperature 40.0 °C
Break
Charpy Impact Unnotched 90.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 95.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 12.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 15.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cm500V; IEC 60093
Surface Resistance 1.00e+12 ohm500V; IEC 60093
Comparative Tracking Index 550 VSol. A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °CISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °CISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 210 °CISO 75/2Af
Vicat Softening Point 215 °C
@Load 5.10 kg
50°C/h; ISO 306
Flammability, UL94 HB
@Thickness 0.800 mm
Flame Spread <= 0.000 mm/min
@Thickness 3.00 mm
Automotive Interior; ISO 3795
Glow Wire Flammability Index 700 °C
@Thickness 2.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 - 280 °C
Mold Temperature 80.0 - 90.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRADICI141 / 313642

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.