MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Copper, UNS C41500, H03 Temper flat products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent cold workability, good hot formability. Fabricated by blanking, drawing, bending, forming, shearing and stamping.

Applications: spring applications for electrical switches.

Test specimen: flat products - 1mm thickness.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 78
Hardness, Rockwell 30T 68
Tensile Strength, Ultimate 435 MPa
Modulus of Elasticity 110 GPaHard
 125 GPaAnnealed
Poissons Ratio 0.28Calculated
Machinability 30 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 46.0 GPa
Shear Strength 290 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000620 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.6 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.380 J/g-°C
Thermal Conductivity 123 W/m-K
@Temperature 20.0 °C
Melting Point 1010 - 1032 °C
Solidus 1010 °C
Liquidus 1032 °C
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 400 - 705 °C
Hot-Working Temperature 730 - 845 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 89 - 93 %
Iron, Fe <= 0.050 %
Lead, Pb <= 0.10 %
Tin, Sn 1.5 - 2.2 %
Zinc, Zn 7.2 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper, UNS C43000, OSO25 Temper flat products
Copper, UNS C42500, OSO25 Temper flat products
Copper, UNS C42200, H02 Temper flat products
Copper, UNS C40800, H08 Temper flat products
Copper, UNS C27000 (Yellow brass), H02 Temper wire

MC41500b7 / 11299

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.