Applications: Automotive: Sun Roof Rails, Fan Shrouds, Air Cleaners, Battery Boxes, Air Induction Components, Battery Trays, Blower Wheels, Light Housings, Shifter Bases, Interior Consoles, Arm Rests Electrical and Industrial: Pool and Spa Pumps and Filters, Small Engine Covers, Air Filter Housings, Cooling Fans, Screens, Lawn Mower Handles, Rotors and Rotary Sprinklers, Large Agricultural Tractors, Roof Liners, Toilet Risers, Cam Stack Timers Information provided by Asahi Kasei |